What causes the deformation of marine propeller blades?
Feb 07, 2023
Due to the long service life of copper propellers, the floating objects collide, hit the rocks or roll into the steel rope, which will cause the blades to deform, and often produce broken blocks and cracks at the same time. After the blade is deformed, the light one will make the pitch error, the heavy one will make the local position of the blade twist or bend and curl near the guide edge and the blade tip outside about 2/3R. The former shall pass the pitch measurement inspection; The latter is often observed directly with the naked eye. The deformation of blades will cause hull vibration, and the tail shaft and tail bearing are easy to wear. The repair of blade bending is often encountered in propeller repair.
The correction methods of blade bending include cold correction and hot correction.
Cold correction refers to the correction carried out under the heating temperature of 205 ℃. The cold correction is applicable to the place where the thickness of blade tip and blade edge is less than 30mm. When the bending is small and the section is thin, the hammer dynamic load can be used for correction, otherwise, the top pressure static load should be used for correction.
Hot correction is suitable for all conditions, mainly used for correction of blade bending degree or large area. Both dynamic and static load correction methods are available. The recommended hot correction temperature shall refer to the preheating temperature of welding repair, and the heating temperature shall pass through the whole section thickness of the correction point and maintain until the correction ends.
The lower support shall be installed at the correction position to avoid transferring the load to other blade sections. Rigid metal pads shall be used for pressure correction. The size of the heating part during blade correction shall be 100-150 mm larger than the part that needs to be corrected, and 50-75 mm from every aspect of the defective part. The correction force shall be determined by considering the physical and mechanical properties of the material in the cold and hot states. After thermal correction, measures must be taken to reduce the cooling speed of the blades by covering the blades with asbestos cloth.